| Grad | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
| Compoziție nominală% | Cr | 12,0-15,0 | 22,0-26,0 | 23,0-26,0 | 19,0-22,0 | 22,5-24,5 | 18,0-21,0 | 21.0-23.0 | 26,5-27,8 |
| Al | 4.0-6.0 | 5.0-7.0 | 4,5-6,5 | 5.0-7.0 | 4,2-5,0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
| Re | oportun | 0,04-1,0 | oportun | oportun | oportun | oportun | oportun | oportun | |
| Fe | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | ||
| Nb0.5 | Mo1.8-2.2 | ||||||||
| Temperatura maximă de funcționare (°C) | 650 | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
| Rezistență 20℃ (Ω/mm2/m) | 1,25 | 1,48 | 1,42 | 1,40 | 1,35 | 1.23 | 1,45 | 1,53 | |
| Densitate (g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7,25 | 7.35 | 7.1 | 7.1 | |
| Conductivitate termică la 20℃, W/(M·K) | 0,49 | 0,49 | 0,46 | 0,48 | 3.46 | 0,49 | 0,49 | 0,49 | |
| Coeficient de dilatare liniară (×10¯6/℃) 20-1000℃) | 15.4 | 16 | 16 | 14 | 15 | 13,5 | 16 | 16 | |
| Punct de topire aproximativ (℃) | 1450 | 1520 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
| Rezistență la tracțiune (N/mm2) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
| Elongaţie(%) | ›16 | ›10 | ›15 | ›15 | ›15 | ›15 | ›15 | ›10 | |
| Rata de contracție a variației secțiunii (%) | 65-75 | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
| Frecvența de curbare repetată (F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | |
| Duritate (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
| Structura micrografică | Ferită | Ferită | Ferită | Ferită | Ferită | Ferită | Ferită | Ferită | |
| Proprietăți magnetice | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | |
| Durată de viață rapidă (h/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 | |